中文   |   English   |   Email Alert

阳极氧化法制备阀金属氧化物纳米管的机理及影响因素

李力成1, 方东1*, 李广忠2, 刘瑞娜1, 刘素琴3, 徐卫林1

化学进展 ›› 2016, Vol. 28 ›› Issue (4) :589-606

PDF (1886KB)
化学进展 ›› 2016, Vol. 28 ›› Issue (4) :589-606 DOI: 10.7536/PC150601
综述与评论
扫码查看或转发全文

阳极氧化法制备阀金属氧化物纳米管的机理及影响因素

    李力成1, 方东1*, 李广忠2, 刘瑞娜1, 刘素琴3, 徐卫林1
作者信息 +

Mechanism and Influence Factors of Valve-Metal Oxide Nanotube Arrays Prepared by Anodization Process

  • Li Licheng1, Fang Dong1*, Li Guangzhong2, Liu Ruina1, Liu Suqin3, Xu Weilin1
Author information +
文章历史 +

摘要

阳极氧化法不仅能够简便地制备出阀金属氧化物纳米管,而且通过调节各种参数可以调控所制备纳米管的形貌.阳极氧化法制备的纳米管具有优异的化学/物理性能,在众多领域都得到了广泛应用.本文综述了阳极氧化法制备纳米管膜的基本过程以及三种常见的模型,并以三种具有代表性的阀金属(Al、Ti、Zr)为例,分别介绍了它们形成多孔膜反应过程和常用的制备过程,同时也介绍了其他阀金属及其合金的制备方案.最后,结合对Al、Ti、Zr的实验过程,讨论、分析了电压大小、电解液种类、电解液浓度、反应时间等控制因素对阳极氧化法制备纳米管膜形貌的影响,对制备形貌规整的多孔膜,提高多孔膜在实际应用中的性能具有一定的意义.

Abstract

The electrochemical anodization method is a simple and versatile process for fabricating well aligned valve-metal oxide nanotube arrays, and the morphology of the nanotube arrays can also be controlled via adjusting the parameters during electrochemical anodization process. Due to their chemical/physical functionality, nanotubes fabricated via electrochemical anodization method have been applied in various fields. The basic formation process of oxide nanotube arrays and three classical models for porous anodic oxide formation are reviewed here. Through the Al, Ti, Zr, which are typical valve-metals, the aim is to illustrate their key processes responsible for the formation of porous anodic oxide film and their general anodic oxidation preparation process. The fabrication methods of other valve-metals even their alloys are reviewed in this paper as well. Furthermore, in combination with the results of the research on Al, Ti, Zr, anodic voltage, electrolyte type, electrolyte concentration, reaction time and so on, which could affect the morphology of the final products, are presented and discussed in detail. The present views may be helpful to adjust the anodization conditions to fabricate well aligned valve-metal oxide nanotube arrays for their extensive applications.

Contents
1 Introduction
2 The basic principle and the common methods of the electrochemical anodization
2.1 The basic principle of the electrochemical anodization
2.2 Preparation of anodic aluminum oxide (AAO)
2.3 Preparation of anodic titanium oxide (ATO)
2.4 Preparation of anodic zirconium oxide (AZO)
3 The essential parameter of electrochemical anodization
3.1 Anodic voltage
3.2 Electrolyte type
3.3 Concentration of the electrolyte
3.4 Reaction time
3.5 Times of anodization
3.6 The metal shape
4 Conclusions

关键词

阳极氧化 / 阀金属 / 影响因素

Key words

anodization / valve metal / effect parameter

引用本文

引用格式 ▾
李力成, 方东, 李广忠, 刘瑞娜, 刘素琴, 徐卫林. 阳极氧化法制备阀金属氧化物纳米管的机理及影响因素[J]. 化学进展, 2016, 28(4): 589-606 DOI:10.7536/PC150601
Li Licheng, Fang Dong, Li Guangzhong, Liu Ruina, Liu Suqin, Xu Weilin. Mechanism and Influence Factors of Valve-Metal Oxide Nanotube Arrays Prepared by Anodization Process[J]. Progress in Chemistry, 2016, 28(4): 589-606 DOI:10.7536/PC150601

登录浏览全文

4963

注册一个新账户 忘记密码

参考文献

[1] Iijima S. Nature, 1991, 354: 56.
[2] Thompson G E, Furneaux R C. Corros. Sci., 1978, 18: 481.
[3] Thompson G E, Wood G C. Nature, 1981, 290: 230.
[4] Chen C C, Chen C L, Lai Y S. Mater. Chem. Phys., 2011, 131: 250.
[5] Miao J Y, Cai Y, Chan Y F, Sheng P, Wang N. J. Phys. Chem. B, 2006, 110: 2080.
[6] Kovtyukhov N I, Martin B R, Mbindyo J K N, Mallouk T E, Cabassi M, Mayer T S. Mater. Sci. Engin. C, 2002, 19: 255.
[7] Zhang Z, Ying J Y, Dresselhaus M S. J. Mater. Res., 1998, 13: 1745.
[8] Johansson A, Torndahl T, Ottosson L M, Boman M, Carlsson J O. Mater. Sci. Eng. C, 2003, 23: 823.
[9] Sui Y C, Acosta D R, Gonzalez-Leon J A, Bermudez A,Feuchtwanger J,Cui B Z,Flores J O,Saniger J M. J. Phys. Chem. B, 2000, 105: 1523.
[10] Luo Z, Fang Y. J. Comb. Chem., 2008, 10: 611.
[11] Choi M K, Yoon H, Lee K, Shin K. Langmuir, 2011, 27: 2132.
[12] Liu L, Yoo S H, Lee S A, Park S. Nano Lett., 2011, 11: 3979.
[13] Zhao X, Lee U J, Lee K H. J. Phys.Chem. C, 2008, 112: 9539.
[14] Papandrew A B, Atkinson R W, Goenaga G A, Kocha S S, Zack J W. J. Electrochem. Soc., 2013, 160: F848.
[15] Santamaria M, Asaro L, Bocchetta P, Megna B, Quarto F D. ECS Electrochem. Lett., 2013, 2: D29.
[16] Kondo T, Miyazaki H, Nishio K, Masuda H. J. Photochem. Photobiol. A, 2011, 221: 199.
[17] Shukla S, Kim K T, Baev A, Yoon Y K, Litchinitser N M, Prasad P N. ACS Nano, 2010, 4: 2249.
[18] Yanagishita T, Nishio K, Masuda H. Appl. Phys. Express, 2008, 1: 067004.
[19] Yanagishita T, Masui M, Ikegawa N, Masuda H. J. Vac. Sci. Technol. B, 2014, 32: 021809.
[20] Yanagishita T, Nishio K, Masuda H. Appl. Phys. Express, 2009, 2: 022001.
[21] Kondo T, Tanji M, Nishio K, Masuda H. Electrochem. Solid-State Lett., 2006, 9: C189.
[22] Lin Q, Hua B, Leung S, Duan X, Fan Z. ACS Nano, 2013, 7: 2725.
[23] Yanagishita T, Nishio K, Masuda H. J. Vac.Sci. Technol. B, 2010, 28: 398.
[24] Yasui K, Morikawa T, Nishio K, Masuda H. Jpn. J. Appl. Phys., 2005, 44: L469.
[25] Liu D, Zhang C, Wang G, Shao Z, Zhu X, Wang N, Cheng H. J. Phys. D: Appl. Phys., 2014, 47: 085108.
[26] Leonardi S, Bassi A L, Russo V, Fonzo F D, Paschos O, Murray T M, Efstathiadis H, Kunze J. J. Phys. Chem. C, 2012, 116: 384.
[27] Vijh A K. Electrodepos. Sur. Treat., 1973, 2: 461.
[28] Mathieu J B, Mathieu H J, Landolt D. J. Electrochem. Soc., 1978, 125: 1039.
[29] Masuda H, Yotsuya M, Asano M, Nishio K, Nakao M, Yokoo A, Tamamura T. Appl. Phys. Lett., 2001, 78: 826.
[30] Spooner R C. J. Electrochem. Soc., 1955, 102: 156.
[31] Sul Y T, Johansson C B, Jeong Y, Albrektsson T. Med. Eng. Phys., 2001, 23: 329.
[32] Habazaki H, Uozumi M, Konno H, Shimizu K, Nagata S, Asami K, Skeldon P, Thompson G E. Electrochem. Acta, 2002, 47: 3837.
[33] Schlotting F, Schreckenbach J, Dietrich D, Hofmann A, Marx G. Appl. Surf. Sci., 1995, 90: 129.
[34] Wang R, Hashimoto K, Fujishima A, Chikuni M, Kojima E, Kitamura A, Shimohigoshi M, Watanabe T. Nature, 1997, 388: 431.
[35] Gratzel M. Nature, 2001, 409: 575.
[36] Chen Q, Peng L M. Inter. J. Nanotechnol., 2007, 4: 44.
[37] Liu J, Cao G, Yang Z, Wang D, Dubois D, Zhou X, Graff G L, Pederson L R, Zhang J. Chem. Sus. Chem., 2008, 1: 676.
[38] Ohtsuka T, Otsuki T. J. Electroanal. Chem., 1999, 473: 272.
[39] Fang D, Huang K L, Liu S Q, Luo Z P, Qing X X,Zhang Q G. J. Alloy. Compd., 2010, 498: 37.
[40] Fang D, Huang K L, Liu S Q, Qin D Y. Electrochem. Comm., 2009, 11: 901.
[41] Fang D, Huang K L, Liu S Q, Li Z J. J. Alloy. Compd., 2008, 464: L5.
[42] Fang D, Huang K L, Liu S Q, Huang J H. J. Braz. Chem. Soc., 2008, 19(6): 1059.
[43] Fang D, Huang K L, Luo Z P, Wang Y, Liu S Q, Zhang Q G. J. Mater. Chem., 2011, 21: 4989.
[44] Zhao J L, Wang X X, Xu R Q, Meng F B, Guo L M, Li Y X. Mater. Lett., 2008, 62: 4428.
[45] Shin Y, Lee S. Nanotechnology, 2009, 20: 105301.
[46] Guo L, Zhao J, Wang X, Xu R, Li Y. J. Solid State Electrochem., 2009, 13: 1321.
[47] Cao W, Tan O K, Zhu W, Jiang B, Reddy C V G. Sensor Actuat. B, 2001, 77: 421.
[48] Cho H J, Choi G M. J. Power Sources, 2008, 176: 96.
[49] Tsai P C, Lee J H, Chang C L. Surf. Coat. Technol., 2007, 202: 719.
[50] Fogaing E Y, Huger M, Gault C. J. Eur. Ceram. Soc., 2007, 27: 1843.
[51] Jin G, Lu G, Guo Y, Guo Y, Wang J, Kong W, Liu X. J. Mol. Catal. A: Chem., 2005, 232: 165.
[52] Bao J, Tie C, Xu Z, Ma Q, Hong J, Sang H, Sheng D. Adv. Mater., 2002, 14: 44.
[53] Shin H J, Jeong D K, Lee J G, Sung M M, Kim J Y. Adv. Mater., 2004, 16: 1197.
[54] Tsuchiya H, Macak J M, Ghicov A, Taveira L, Schmuki P. Corros. Sci., 2005, 47: 3324.
[55] Thormann A, Teuscher N, Pfannmcller M, Rothe U, Heilmann A. Small, 2007, 3 (6): 1032.
[56] Matsumotoa F, Nishioa K, Masuda H, Electrochem. Soc. Inc., 2004: 204.
[57] Mor G K, Shankar K, Paulose M K, Varghese O A, Grimes C. Nano Lett., 2006, 6: 215.
[58] Bauer S, Prak J, Faltenbacher S, Berger K P, Schmuki V. Integr. Biol., 2009, 1: 525.
[59] Bavykin D V, Friedrich J M, Walsh F C. Adv. Mater., 2006, 18: 2807.
[60] Su Z X, Zhou W Z. J. Mater. Chem., 2011, 21: 8955.
[61] Poinern G E J, Ali N, Fawcett D. Materials, 2011, 4: 487.
[62] Ghicov A, Schmuki P. Chem. Comm., 2009, 20: 2791.
[63] Pang Y L, Lim S, Ong H C, Chong W T. Appl. Catalysis A: General, 2014, 481: 127.
[64] Zhou X M, Nguyen N T, Ozkan S, Schmuki P. Electrochem. Comm., 2014, 46: 157.
[65] Jarosz M, Pawlik A, Kapusta-Koodziej J, Jaskua M, Sulka G D. Electrochem. Acta, 2014, 136: 412.
[66] Zhuang H F, Lin C J, Lai Y K. Environ. Sci. Technol., 2007, 41: 4735.
[67] Shankar K, Basham J, Allam N K, Varghese O K, Mor G K, Feng X J, Paulose M, Seabold J A, Choi K S, Grimes C A. J. Phys. Chem. C, 2009, 113(16): 6327.
[68] Chen C C, Fang D, Luo Z P. Rev. Nanosci. Nanotechnol., 2012, 1: 229.
[69] 黄奇松(Huang Q S). 铝的阳极氧化和染色(Anodic Qxidation and Staining of Aluminum). 香港:香港万里出版社(Hongkong:Hongkong Wan Li Press), 1985.
[70] Mor G K, Varghese O K, Paulose M, Shankar K, Grimes C A, Sol. Energy Mater. Sol. Cells, 2006, 90: 2011.
[71] Taveira L V, Macak J M, Tsuchiya H, Dick L F P, Schmuki A P, J. Electrochem. Soc., 2005, 152: B405.
[72] Daskf C, Caterry H. Corros. Sci., 1987, 27(1): 83.
[73] Jessensky O, Muller F, Gosele U. Appl. Phys. Lett., 1998, 72(10): 1173.
[74] Xu Y, Thompson G E, Wood G C, Trans. Inst. Met. Finish., 1985, 63: 98.
[75] Chen S H, Chen C C, Luo Z P, Chao C G. Mater. Lett., 2009, 63: 1665.
[76] Say W C, Chen C C. Jpn. J. Ceramic Soc., 2008, 116: 288.
[77] Say W C, Chen C C. Jpn. J. Appl. Phys., 2007, 46: 7577.
[78] Chen C C, Bisrat Y, Luo Z P, Schaak R E, Chao C G, Lagoudas D C. Nanotechnolo., 2006, 17: 367.
[79] Chen C C, Chen J H, Chao C G. Jpn. J. Appl. Phys., 2005, 44: 1529.
[80] Chen C C, Kuo C G, Chen J H, Chao C G. Jpn. J. Appl. Phys., 2004, 43: 8354.
[81] Zwilling V, Aucouturier M, Ceretti E D, Electrochim. Acta, 1999, 45: 921.
[82] Cai Q, Paulose M, Varghese O K, Grimes C A. J. Mater. Res., 2005, 20: 230.
[83] Grimes C A. J. Mater. Chem., 2007, 17: 1451.
[84] Paulose M, Shankar K, Yoriya S, Prakasam H E, Varghese O K, Mor G K, Latempa T A, Fitzgerald A, Grimes C. A. J. Phys. Chem. B, 2006, 110: 16179.
[85] Yetim A F. Surf. Coat. Tech., 2010, 205: 1757.
[86] Lim J H, Choi J. Small, 2007, 3: 1504.
[87] Tao J, Zhao J, Wang X, Kang Y, Li Y. Electrochem. Comm., 2008, 10: 1161.
[88] Kim D, Stein F S, Hahn R, Schmuki P. Electrochem. Comm., 2008, 10: 1082.
[89] Pouporte T, Finne J. J. Appl. Electrochem., 2006, 36: 33.
[90] Khalil N, Leach J S. J. Appl. Electrochem., 1996, 26: 231.
[91] Tsuchiya H, Schmuki P. Electrochem. Comm., 005, 7: 249.
[92] Maeng S, Axe L, Tyson T. J. Electrochem. Soc., 2005, 152: B60.
[93] Tsuchiya H, Macak J M, Sieber I, Taveira L, Ghicov A, Sirotna K, Schmuki P. Electrochem. Comm., 2005, 7: 295.
[94] Yoo J E, Park J Y, Cha G, Choi J. Thin Solid Films, 2013, 531: 583.
[95] Yu L G, Zhang G M, Zhao X Y, Guo D Z. Mater. Res. Bull., 2009, 44: 589.
[96] Jeun J H, Ryu H S, Hong S H. J. Electrochem. Soc., 2009, 156(9): J263.
[97] Albu S P, Ghicov A, Schmuki P. Phys. Status Sol. RRL 3, 2009, 2(3): 64.
[98] Yang Y, Albu S P, Kim D, Schmuki P. Angew. Chem. Int. Ed., 2011, 50: 9071.
[99] Lee C Y, Lee K Y, Schmuki P. Angew. Chem. Int. Ed., 2013, 52: 2077.
[100] Semboshi S, Bando K I, Ohtsu N, Shim Y, Konno T J. Thin Solid Films, 2008, 516: 8613.
[101] Lewandowska M, Pisarek M, Rozniatowski K, Gradzka-Dahlke M, Janik-Czachor M, Kurzydiowski K J. Thin Solid Films, 2007, 515(16): 6460.
[102] Li M F, Zhao G H, Liu M C, Lei Y Z, Jin Y N, Li D M. Electrochem. Comm., 2011, 13: 942.
[103] Simka W. Electrochim. Acta, 2011, 56: 9831.
[104] Ohtsua N, Masahashib N, Mizukoshi Y. Appl. Surf. Sci., 2012, 258: 6052.
[105] Oliveira N T C, Guastaldi A C. Corros. Sci., 2008, 50: 938.
[106] Paez M A, Skeldon R, Thompson G E, Saez M, Bustos O, Monsalve A. Rev. Metal. MadridVol. Extr., 2003, 243: 243.
[107] Kikuchi T, Haraa Y, Sakairi M, Yonezawa T, Yamauchi A,Takahashi H. Corros. Sci., 2010, 52: 2525.
[108] Regone N N, Freire C M A, Ballester M. J. Mater. Pro. Tech., 2006, 72: 146.
[109] Nagai A, Suzuki Y, Tsutsμmi Y, Nozaki K, Wada N, Katayama K, Hanawa T, Yamashita K. Mater. Res. Part B, 2014, 102: 659.
[110] Moon S M, Nam Yunk Y. Corros. Sci., 2012, 65: 494.
[111] Keller F, Hunter M S, Robinson D L. J. Electrochem. Soc., 1953, 100(9): 411.
[112] O'Sullivan J P, Wood G C. Proc. R. Soc. London A, 1970, 317: 511.
[113] Heber K V. Electrochem. Acta, 1978, 23(2): 135.
[114] Thompson G E, Wood G C. Corrososion: Aqueous Processed and Passive Films, 1983, 23: 205.
[115] Young L. Anodic Oxide Films. New York:Academic Press, 1961: 116.
[116] 方东(Fang D). 中南大学博士论文(Doctoral Dissertation of Central South University). 2011.
[117] Fang D, Luo Z P, Liu S Q, Zeng T F, Liu L, Xu J, Bai Z K, Xu W L. Opt. Mater., 2013, 35: 1461.
[118] Fang D, Liu S Q, Luo Z P, Xiong C X, Xu W L. Appl. Surf. Sci., 2012, 258: 6217.
[119] Parkhutik V P, Shershulsky V I. J. Phys. D:Appl. Phys., 1992, 25: 1258.
[120] Diggle J W, Downie T C, Goulding C W. Chem. Rev., 1969, 69: 365.
[121] Chen W, Wang F B, Ruan M H. Sci. Adv. Mater., 2009, 1: 25.
[122] Su Z X, Hahner G, Zhou W Z. J. Mater. Chem., 2008, 18: 5787.
[123] Yuan J H, Chen W, Hui R J, Hu Y L, Xia X H. Electrochim. Acta, 2006, 51: 4589.
[124] Jo Y, Jung I, Lee I, Choi J, Tak Y. Electrochem. Comm., 2010, 12: 616.
[125] Furneaux R C, Rigby W R, Davidson A P. Nature, 1989, 337: 147.
[126] Macak J M, Tsuchiya H, Ghicov A, Yasuda K, Hahn R, Bauer S, Schmuki P. Solid State Mater. Sci., 2007, 11: 3.
[127] Yin A J, Guico R S, Xu J. Nanotechnolo., 2007, 18: 35304.
[128] Thompson G E. Thin Solid Films, 1997, 297: 192.
[129] Parkhutik V P, Despic A. Springer US: Modern Aspects of Electrochemistry, 1989, 20: 401.
[130] Shingubara S. J. Nanoparticle Res., 2003, 5: 17.
[131] Ono S, Masuko N. J. Surf. Coat Tech., 2003, 169/170: 139.
[132] Jagminience A, Valincius G, Riaukaite A, Jagminas A. J. Cryst. Growth Des., 2005, 274: 622.
[133] Wood G C, O'Sullivan J P, Vaszko B. J. Electrochem. Soc., 1968, 115: 618.
[134] Li A P, Muller F, Birner A, Gosele U. J. Appl. Phys., 1998, 84: 6023.
[135] Vrublevsky I, Parkoun V, Schreckenbach J. Appl. Surf. Sci., 2005, 242(3/4): 333.
[136] Azevedo W M, Carvalho D D, Khoury H J, Vasconcelos E A, Silva E F. Mater. Sci. Eng. B, 2004, 112: 171.
[137] Suh J S, Lee J S. Appl. Phys. Lett., 1999, 75: 2047.
[138] Sulka G D, Parkola K. Thin Solid Films, 2006, 515: 338.
[139] Prasad S, Quijano. Bioelectronics, 2006, 7: 1219.
[140] Domanska M M, Norek M, Stepniowski W J, Budner B. Electrochim. Acta, 2013, 105: 424.
[141] Zhou X, Thompson G E, Potts G. Trans. Inst. Met. Finish, 2000, 78: 210.
[142] Sadasivan V, Richter C P, Menon L, Williams P F. AIChE J., 2005, 51: 649.
[143] Stepniowski W J, Domanska M, Norek M, Czujko T. Mater. Lett., 2014, 117: 69.
[144] Stepniowski W J, Norek M, Michalska-Domanska M, Bombalska A, Nowak-Stepniowska A, Kwasny M, Bojar Z. Appl. Surf. Sci., 2012, 259: 324.
[145] Nishinaga O, Kikuchi T, Natsui S, Suzuki R O. Sci. Rep., 2013, 3: 2748.
[146] Kikuchi T, Nishinaga O, Natsui S, Suzuki R O. Electrochim. Acta, 2014, 137: 728.
[147] Flamme K E, Popat K C, Leoni L, Markiewicz E, Tempa T J, Roman B B, Grimes C A, Desai T A. Biomaterials, 2007, 28: 2638.
[148] Kim Y, Jung B, Lee H, Kim H, Lee K, Park H. Actuator. B, 2009, 141: 441.
[149] Ng K Y, Lin Y, Ngan A H W. J. Mech. Phys. Solids, 2011, 59: 251.
[150] Zhao Y, Chen M, Zhang Y, Xu T, Liu W. Mater. Lett., 2005, 59: 40.
[151] Wang X, Han G. Microelectron Eng., 2003, 66: 166.
[152] Zhao N Q, Jiang X X, Shi C S, Li J J, Zhao Z G, Du X W. J. Mater. Sci., 2006, 42: 3878.
[153] Larsson C, Thomsaon P, Aronsson B O, Rodahl M, Lausmaa J, Kasemo B, Erison L E. Biomaterials, 1996, 17: 605.
[154] Chu S Z, Wada K, Inoue S, Isogai M, Katsuta Y, Yasumori A. J. Electrochem. Soc., 2006, 153: B384.
[155] Mozalev A, Mozaleva I, Sakairi M, Takahashi H. Electrochim. Acta, 2005, 50: 5065.
[156] Tajima S, Baba N, Shimizu K, Mizuki I. Electrocomp. Sci. Tech., 1976, 3: 91.
[157] Bellemare J, Sirois F, Menard D. J. Electrochem. Soc., 2014, 161: E75.
[158] Kikuchi T, Yamamoto T, Suzuki R O. Appl. Surf. Sci., 2013, 284: 907.
[159] Ono S, Saito M, Asoh H. Electrochim. Acta, 2005, 51: 827.
[160] Sun B, Li J, Jin X, Zhou C Q, Hao Q L, Gao X F, Electrochim. Acta, 2013, 112: 327.
[161] Vrublevsky I A, Chernyakova K V, Ispas A, Bund A, Zavadski S. Thin Solid Films, 2014, 556: 230.
[162] Pashchanka M, Schneider J. Phys. Chem., 2013, 15: 7070.
[163] Kikuchi T, Nishinaga O, Natsui S, Suzuki R O. ECS Electrochem. Lett., 2014, 3: C25.
[164] Kikuchi T, Yamamoto T, Natsui S, Suzuki R O. Electrochim. Acta, 2014, 123: 14.
[165] Kikuchi T, Nakajima D, Kawashima J, Natsui S, Suzuki R O. Appl. Surf. Sci., 2014, 313: 276.
[166] Gong D, Grimes C A, Varghese O K, Hu W, Singh R S, Chen Z, Dickey E C. J. Mater. Res., 2001, 16: 3331.
[167] Ruan C, Paulose M, Varghese O K, Grimes C A. Sol. Ener. Mater. Sol. Cells, 2006, 90: 1283.
[168] Lockman Z, Ismail S, Sreekantan S, Mende L S, Driscoll J L M. Nanotechnology, 2010, 21: 055601.
[169] Nakayama K, Kubo T, Tsubokura A, Nishikitani Y, Masuda H. ECS Meeting Abstracts, 2006, 502: 819.
[170] Richter C, Wu Z, Panaitescu E, Willey R J, Menon L. Adv. Mater., 2007, 19: 946.
[171] Richter C, Panaitescu E, Willey R J, Menon L. J. Mater. Res., 2007, 22: 1624.
[172] Ruan C, Paulose M, Varghese O K, Mor G K, Grimes C A. J. Phys. Chem. B, 2005, 109: 15754.
[173] Macak J M, Tsuchiya H, Taveira L, Aldabergerova S, Schmuki P. Angew. Chem., Int. Ed., 2005, 44: 7463.
[174] Shankar K, Mor G K, Prakasam H E, Yoriya S, Paulose M, Varghese O K, Grimes C A. Nanotechnology, 2007, 18: 065707.
[175] Ghicov A, Tsuchiya H, Macak J M, Schmuki P. Electrochem. Commun., 2005, 7: 505.
[176] Macak J M, Sirotna K, Schmuki P. Electrochim. Acta, 2005, 50: 3679.
[177] Sreekantan S, Lockman Z, Hazan R, Tasbihi M, Tong L K, Mohamed A R. J.Alloys Compd., 2009, 485: 478.
[178] Tsuchiya H, Macak J M, Taveira L, Balaur E, Ghicov A, Sirotna K, Schmuki P. Electrochem. Commun., 2005, 7: 576.
[179] Liu Z, Liu H, Hashimoto T, Thompson G E, Skeldon P. Mater. Charact., 2014, 98: 102.
[180] Roman I, Trusca R D, Soare M L, Fratila C, Krasicka-Cydzik E, Stan M S, Dinischiotu A. Mater. Sci. Eng. C, 2014, 37: 374.
[181] Nischk M, Mazierski P, Gazda M, Zaleska A. Appl. Catal. B, 2014, 144: 674.
[182] Antony R P, Mathews T, Ramesh C, Murugesan N, Dasgupta A, Dhara S, Dash S, Tyagi A K. Int. J. Hydrogen Energy, 2012, 37: 8268.
[183] Jha H, Roy P, Hahn R, Paramasivam I, Schmuki P. Electrochem. Commun., 2011, 13: 302.
[184] Tsuchiya H, Macak J M, Sieber I, Schmuki P. Small, 2005, 1: 722.
[185] Wang L N, Shen C, Shinbine A, Luo J L. Thin Solid Films, 2013, 531: 277.
[186] Ali G, Park Y J, Kim H J, Sung O C. Nanoscale Res. Lett., 2014, 9(1): 553.
[187] Muratore F, Baron-Wieche? A, Gholinia A, HashimotoT, Skeldon P, Thompson G E. Electrochim. Acta, 2011, 58: 389.
[188] Wang L N, Luo J L. Mater. Sci. Eng. C, 2011, 31(4): 748.
[189] Belwalkar A, Grasing E, Geertruyden W V, Huang Z, Misiolek W Z. J. Memb. Sci., 2008, 319(1/2): 192.
[190] Chung C K, Liu T Y, Chang W T. Microsyst. Technol., 2010,16: 1451.
[191] Huang B, Guo Y F, Tian Y L, Wen Y W, Shan B, Chen R. ECS, 2013, 50: 279.
[192] Fang D, Chen S S, Jiang M, Li Q, Luo Z P, Liu L, Xiong C X. Mater. Sci. Semicon. Proc., 2014, 18: 105.
[193] Fang D, Yu J G, Luo Z P, Liu S Q, Huang K L, Xu W L. J. Solid State Electrochem., 2012, 16: 1219.
[194] Fang D, Li L C, Xu W L, Wang Y L, Jiang M, Guo X Q, Liu X, Cao G Y, Li G Z, Gang L B, Wang N F, Luo Z P. Mater. Sci. Eng. B, 2014, 179: 71.
[195] Masuda H, Yada K, Osaka A. Jpn. J. Appl. Phys., 1998, 37: L1340.
[196] Masuda H, Satoh M. Jpn. J. Appl. Phys., 1996, 35: L126.
[197] Bi Z H, Parans P M, Menchhofer P A, Dehoff R R, Bridges C A, Chi M F, Guo B K, Sun X G, Dai S. J. Power Sources, 2013, 222: 461.
[198] Yu J F, Wang D, Huang Y N, Fan X, Tang X, Gao C, Li J L, Zou D C, Wu K. Nanoscale Res. Lett., 2011, 6: 94.
[199] Chen T, Qiu L B, Yang Z B, Cai Z B, Ren J, Li H P, Lin H J, Sun X M, Peng H S. Angew. Chem. Int. Ed., 2012, 51: 11977.
PDF (1886KB)

2939

访问

0

被引

详细

导航
相关文章

/

〈 〉