挥发性有机物(VOCs)是一类具有毒性且对环境和人体健康产生威胁的有机化合物。目前催化氧化技术是有效净化VOCs的方法之一,它可以将VOCs转化为CO2和H2O。本文在总结国内外VOCs净化技术的基础上,着重介绍了催化氧化技术,并且对常用的催化剂种类、催化机理及存在的问题进行了总结。最后对催化氧化技术的发展趋势进行了展望。研究结果表明,贵金属催化剂的研究关键在于有效载体的选择及催化剂抗中毒性能的提高;与贵金属催化剂相比,钙钛矿和尖晶石等非贵金属催化剂的发展趋势为通过改变催化剂配方、催化剂形貌结构、活性组分粒径大小及比表面积等来提高催化剂的低温可还原性、储氧能力和氧缺陷,进而提高其催化性能。本文的评述将为选择合适的催化剂处理VOCs提供一定的参考基础。
[1] Hutchings G J, Heneghan C S, Hudson I D, Taylor S H. Nature, 1996, 384:341.
[2] Le Cloirec P. Rev. Environ. Sci. Bio., 2012, 11(4):381.
[3] Atkinson R, Arey J. Chem. Rev., 2003, 103(12):4605.
[4] Yu C, Crump D. Build. Environ., 1998, 33(6):357.
[5] Tchobanoglous G, Theisen H, Vigil S. Integrated Solid Waste Management:Engineering Principles and Management Issues. NY:McGraw-Hill, Inc., 1993. 80
[6] 杨新兴(Yang X X), 李世莲(Li S L), 尉鹏(Wei P), 冯丽华(Feng L H).前沿科学(Frontier Science), 2013, 7(4):21.
[7] 王连生(Wang L S). 高等教育出版社(Higher Education Press), 2004, 122.
[8] Mølhave L, Bach B, Pedersen O F. Environ. Int., 1986, 12:167.
[9] World Health Organization (WHO). Air quality guidelines for Europe, 2nd edition. European Series, No.91. WHO Regional Publications, 2000.
[10] 张薇薇(Zhang W W). 大连理工大学硕士论文(Master's Dissertation of Dalian University of Technology), 2011.
[11] 孟中华(Meng Z H). 浙江大学硕士论文(Master's Dissertation of Zhejiang University), 2013.
[12] Roizard D, Lapicque F, Favre E, Roizard C. Chem. Eng. Sci., 2009, 64(9):1927.
[13] Yu C, Crump D. Build. Environ., 1998, 33(6):357.
[14] Müller G, Ulrich M. Chem. Ing. Tech., 1991, 63(8):819.
[15] Trimm D L. Appl. Catal., 1983, 7(3):249.
[16] Tsuru T, Kanno T, Yoshioka T, Asaeda M. J. Membrane Sci., 2006, 280(1):156.
[17] Rusu A O, Dumitriu E. Environ. Eng. Manag. J., 2003, 2(4):273.
[18] Spivey J J. Ind. Eng. Chem. Res., 1987, 26(11):2165.
[19] Scirè S, Liotta L F. Appl. Catal. B:Environ., 2012, 125:222.
[20] Everaert K, Baeyens J. J. Hazard. Mater., 2004, 109(1):113.
[21] Mukadi L S, Hayes R E. Comput. Chem. Eng., 2002, 26(3):439
[22] Stoyanova M, Konova P, Nikolov P, Naydenov A, Mehandjiev D. Chem. Eng. J., 2006, 122(1):41.
[23] Alvarez-Merino M A, Ribeiro M F, Silva J M,Carrasco-Marin F, Maldonado-Hodar F J. Environ. Sci. Technol., 2004, 38(17):4664.
[24] Balasubramanian S, Viswanath D S. Ind. Eng. Chem. Res., 1975, 14(3):158.
[25] Grasselli R K. Top. Catal., 2002, 21(1/3):79.
[26] Tang W X, Wu X F, Li D Y, Wang Z, Liu G, Liu H D, Chen Y F. J. Mater. Chem. A, 2014, 2:2544.
[27] Akram S, Wang Z, Chen L, Wang Q, Shen G L, Han N, Chen Y F, Ge G L. Catal. Communi., 2016, 73:123.
[28] Liotta L F. Appl. Catal. B:Environ., 2010, 100(3):403.
[29] Tidahy H L, Hosseni M, Siffert S, Cousin R, Lamonier J F, Aboukaïs A, Su B L, Giraudon J M, Leclercq G. Catal. Today, 2008, 137(2):335.
[30] Lewandowski M, Ollis D F. J. Catal., 2003, 217:38.
[31] Ousmane M, Liotta L F, Di Carlo G, Pantaleo G, Venezia A M, Deganello G, Retailleau L, Boreave A, Giroir-Fendler A. Appl. Catal. B:Environ., 2011, 101(3):629.
[32] Lamallem M, El Ayadi H, Gennequin C, Cousin R, Siffert S, Aïssi F, Aboukaïs A. Catal. Today, 2008, 137(2):367.
[33] Gluhoi A C, Bogdanchikova N, Nieuwenhuys B E. J.Catal., 2005, 229(1):154.
[34] Tan W, Guo G, Deng J, Xie S, Yang H, Jiang Y, Dai H. Ind. Eng. Chem. Res., 2014, 53(48):18452.
[35] Han W, Deng J, Xie S, Yang H, Dai H, Au C T. Ind. Eng. Chem. Res., 2014, 53(9):3486.
[36] Cellier C, Lambert S, Gaigneaux E M, Poleunis C, Ruaux V, Eloy P, Lahousse C, Bertrand P, Pirard J P, Grange P. Appl. Catal. B:Environ., 2007, 70(1):406.
[37] Carabineiro S A C, Chen X, Martynyuk O, Bogdanchikova N, Avalos-Borja M, Pestryakov A, Tavares P B, Órfão J J M, Pereira M F R, Figueiredo J L. Catal. Today, 2015, 244:103.
[38] Huang S, Zhang C, He H. Catal. Today, 2008, 139(1):15.
[39] He C, Li J, Zhang X, Yin L, Chen J, Gao S. Chem. Eng. J., 2012, 180:46.
[40] Wang Y, Zhang C, Liu F, He H. Appl. Catal. B:Environ., 2013, 142:72.
[41] Wu Z X, Deng J G, Xie S H, Yang H G, Zhao X T, Zhang K F, Lin H X, Dai H X, Guo G S. Micropor. Mesopor. Mat., 2016, 224:311.
[42] Paulis M, Peyrard H, Montes M. J. Catal., 2001, 199(1):30.
[43] Tang W, Wu X, Chen Y. React. Kinet. Mech. Cat., 2015, 114(2):711.
[44] Li Z H, Yang K, Liu G, Deng G F, Li J Q, Li G, Yue R L, Yang J, Chen Y F. Catal. Let., 2014, 144(6):1080.
[45] Deng J, He S, Xie S, Yang H, Liu Y, Guo G, Dai H. Environ. Sci. Technol., 2015, 49(18):11089.
[46] Giraudon J M, Elhachimi A, Wyrwalski F, Siffert S, Aboukais A, Lamonier J F, Leclercq G. Appl. Catal. B:Environ., 2007, 75(3):157.
[47] Papaefthimiou P, Ioannides T, Verykios X E. Appl. Catal. B, 1997, 13:175.
[48] Fiorenza R, Crisafulli C, Condorelli G G, Lupo F, Scirè S. Catal. Lett., 2015, 145(9):1691.
[49] Baek S W, Kim J R, Ihm S K. Catal. Today, 2004, 93:575.
[50] Tidahy H L, Siffert S, Lamonier J F, Zhilinskaya E A, Aboukaïs A, Yuan Z Y, Vantomme A, Su B L, Canet X, Deweireld G, Frère M N, Guyen T B, Giraudon J M, Leclercq G.Appl. Catal. A:Gen., 2006, 310:61.
[51] Tidahy H L, Siffert S, Lamonier J F, Zhilinskaya E A, Aboukais A, Yuan Z Y, Vantomme A, Su B L, Canet X, Deweireld G, Frere M. Stud. Surf. Sci. Catal., 2007, 160:201.
[52] Pozan G S. J.Hazard. Mater., 2012, 221:124.
[53] Tang W X, Deng Y Z, Li W H, Li J Q, Li G, Li A D, Wu X F, Chen Y F. Catal. Sci. Technol., 2016, 6(6):1710.
[54] Njagi E C, Genuino H C, King'ondu C K, Dharmarathna S, Suib S L. Appl. Catal. A:Gen., 2012, 421:154.
[55] Dai Q, Wang X, Lu G. Appl. Catal. B:Environ., 2008, 81(3):192.
[56] Pérez A, Molina R, Moreno S. Appl. Catal. A:Gen., 2014, 477:109.
[57] de Rivas B, López-Fonseca R, Jiménez-González C, Gutiérrez-Ortiz J I. J. Catal., 2011, 281(1):88.
[58] Wang F, Dai H, Deng J, Bai G, Ji K, Liu Y. Environ. Sci. Technol., 2012, 46(7):4034.
[59] Cao S, Wang H Q, Yu F X, Shi M P, Chen S, Weng X L, Liu Y, Wu Z B. J. Colloid Interf. Sci., 2016, 43:233.
[60] Wei Y C, Liu J, Zhao Z, Duan A J, Jiang G Y, Xu C M, Gao J S, He H, Wang X P. Energy Environ. Sci., 2011, 4(8):2959.
[61] He C, Yu Y K, Chen C W, Yue L, Qiao N L, Shen Q, Chen J S, Hao Z P. RSC Adv., 2013, 3(42):19639.
[62] Du Y C, Meng Q, Wang J S, Yan J, Fan H G, Liu Y X, Dai H X. Micropor. Mesopor. Mat., 2012, 162:199.
[63] Tang W X, Wu X F, Li S D, Shan X, Liu G, Chen Y F. Appl. Catal. B:Environ., 2015, 162:110.
[64] Zhang H M, Shimizu Y, Teraoka Y, Miura N, Yamazoe N. J. Catal., 1990, 121(2):432.
[65] Rezlescu N, Rezlescu E, Popa P D, Doroftei C, Ignat M. Mater. Chem. Phys., 2016, 182:332.
[66] Luo Y, Wang K, Chen Q, Xu Y, Xue H, Qian Q. J. Hazar. Mater., 2015, 296:17.
[67] Zhang J Y, Tan D D, Meng Q J, Wen X L, Wu Z B. Appl. Catal. B:Environ., 2015, 172:18.
[68] 王永强(Wang Y Q), 肖丽(Xiao L), 孙启猛(Sun Q M), 赵朝成(Zhao C C), 李石(Li S). 燃烧化学学报(Journal of Fuel Chemistry and Technology). 2014, 9(42):1146.
[69] Hosseini S A, Salari D, Niaei A, Oskoui S. J. Ind. Eng. Chem., 2013, 19:1903.
[70] Rezlescu N, Rezlescu E, Popa P D, Doroftei C, Ignat M. Ceram. Internat., 2015, 41(3):4430.
[71] Liu Y X, Dai H X, Du Y C, Deng J, Zhang L, Zhao Z, Au C T. J. Catal., 2012, 287:149.
[72] Ji K M, Dai H X, Dai J X, Deng J G, Wang F, Zhang H, Zhang L. Catal. Today, 2013, 201:40.
[73] Ji K M, Dai H X, Deng J G, Jiang H Y, Zhang L, Zhang H, Cao Y J. Chem. Eng. J., 2013, 214:262.
[74] Gao B Z, Deng J G, Liu Y X, Zhao Z X, Li X W, Wang Y, Dai H X. Chinese J. Catal., 2013, 34(12):2223.
[75] Chen Y W, Li B, Niu Q, Li L, Kan J W, Zhu S M, Shen S B. Environ. Sci. Pollut. Res., 2016, 23:15193.
[76] Jiang Y, Deng J G, Xie S H, Yang H G, Dai H X. Ind.Eng.Chem.Res., 2015, 54(3):900.
[77] Li X W, Dai H X, Deng J G, Liu Y X, Xie S H, Zhao Z X, Wang Y, Guo G S, Hamidreza Arandiyan. Chem.Eng. J., 2013, 228(14):965.
[78] Yong S T, Hidajat K, Kawi S. Catal. Today, 2008, 131(1):188.
[79] Hosseini S A, Niaei A, Salari D, Nabavi S R. Ceram Int., 2012, 38(2):1655.
[80] Hosseini S A, Salari D, Niaei A, Deganello F, Pantaleo G, Hojati P. J. Environ. Sci. Heal. A, 2011, 46(3):291.
[81] Li D L, Fan Y Y, Ding Y Y, Wei X F, Xiao Y H. Catal. Commun., 2017, 88(5):60.
[82] Alphonse P. Appl. Catal. B:Environ., 2016, 180:715.
[83] Zav'yalova U, Nigrovski B, Pollok K, Langenhorst F, Müller B, Scholz P, Ondruschka B. Appl. Catal. B:Environ., 2008, 83(3):221.
[84] Castillo S, Moran-Pineda M, Gómez R, López T. J. Catal., 1997, 172(1):263.
[85] Vodyankin A Y, Kurina L N, Popov V N. Kinetika i kataliz, 1999, 40(4):636.
[86] Hosseini S A, Niaei A, Salari D, Nabavi S R. Ceram. Int., 2012, 38(2):1655.
[87] Tang Q H, Wu C M, Qiao R, Chen Y T, Yang Y H. Appl. Catal. A:Gen., 2011, 403(1):136.
[88] Jodaei A, Salari D, Niaei A, Khatamian M, Ali Hosseini S. J. Environ. Sci. Heal. A, 2011, 46(1):50.
[89] Chen M, Zheng X M. J. Mol. Catal. A:Chem., 2004, 221(1):77.
[90] Garetto T F, Vignatti C I, Borgna A, Monzón A. Appl. Catal. B:Environ., 2009, 87(3):211.
[91] Ran L, Qin Z, Wang Z, Wang X, Dai Q. Catal. Commun., 2013, 37:5.
[92] Zhao S, Li K Z, Jiang S, Li J H. Appl. Catal. B:Environ., 2016, 181:236.
[93] Zawadaki M, Okal J. Catal. Today, 2015, 257:136.
[94] Tian Z Y, Ngamou P H T, Vannier V, Kohse-Höinghaus K, Bahlawane N. Appl. Catal. B:Environ., 2012, 117(3):125.
[95] 余凤江(Yu F J), 张丽丹(Zhang L D). 北京化工大学学报:自然科学版(Journal of Beijing University of Chemical Technology), 2001, 28(4):67.
[96] Groppi G, Cristiani C, Forzatti P. Appl. Catal. B:Environ., 2001, 35(2):137.